What's New here?
Updated 8/5/08


Welcome to ThinBoards.com

Skip Navigation Links
Home
How To Order
About Us

eMail me
Wood designed for scrolling, intarsia, inlay, and general woodworking.

Skip Navigation Links
Thin Boards 1/8" & thickerExpand Thin Boards 1/8" & thicker
Thin Boards (Veneer)Expand Thin Boards (Veneer)
Thuya Boxes (Humidors)Expand Thuya Boxes (Humidors)
Pen Blanks & Pool CuesExpand Pen Blanks & Pool Cues
Bowl BlanksExpand Bowl Blanks
Anchorseal
Variety Packs of Craft WoodExpand Variety Packs of Craft Wood
Wood Photos
Species AvailableExpand Species Available
Customer ShowcaseExpand Customer Showcase
Tree FacesExpand Tree Faces

Bleaches in Woodworking
Picking Your Finish
Purpleheart's Purple
How To Apply A Wood Finish
This is a 1 gallon jug of a Anchorseal wax emulsion.

I offer a full money back guarantee, if not fully satisfied.

Buy with confidence.

Priced at $19.95 per gallon.

 

See for yourself, the difference above is a log that had no wax emulsion, and one that did.

 

BENEFITS --- stops most end checking before it begins. The sooner end sealer is applied, the more effective it will be. Depending on the species, 5 - 20% of your logs and lumber can be saved by using immediately after sawing.

SUPERIOR QUALITY --- is known in the forest products industry as the best quality sealer and most stable wax emulsion coating available. For over two decades, it has been the sealer of choice in the hardwood industry.

PROVEN RESULTS --- Independent studies* have concluded that end coating has great benefit by reducing degrade. In freshly sawn lumber it reduces end checking losses. In freshly cut logs, it reduces blue stain and end checking.

 

APPLICATION

1. Apply as soon as possible after cutting or end trimming, to all end grain surfaces. On valuable veneer logs, areas where bark is removed should also be treated.
2. Apply with a brush, roller, or with spray equipment. If a sprayer is used, the tip must be large enough to accommodate the thick emulsion.
3. Valuable logs will benefit from a heavy application. Logs under 24"/60cm can be coated "to the drip". Logs over 24"/60 cm should be coated very heavily, perhaps twice within 15 minutes. The increase in value/yield from the larger logs will be worth the little extra time and wax used.